Hi All,

Looking for some guidance on the best materials to use for Sulfuric Acid pipework transfer, and diluted but low pH mixture. There are two operating conditions:

1) 98% Sulfuric Acid injection to a tank - ambient temp but tank is heated w/steam to approx 90-100 deg C therefore can consider some heat transfer, particularly at the connection point/flange
2) Highly acidic (pH 2) Acid Water and Acid Oil pipelines (following injection of H2S04) at 100 deg C, roughly 5% dilution of sulfuric acid in the mix.

Pipeline velocities <2m/s

For background info the application is an oil soapstock splitting plant

Appreciate any help
 
It would be helpful if you could determine to what extent heat transfer will occur? I assume it is ambient initially?

How much cost consideration is going into this?
 