Hello..experts,

Liquid sulfur from the Refinery is processed in Rotoform to produce sulfur pastill ,min.spec of crushing strength of 3.5 kg/cm2g ,liquid sulfur temp. remains 122 -125 C , C.W.Flow is ~ 35 m3/hr --indirect cooling below the belt.however..crushing strength is not able to meet the specs...is there any way..to rectify the problem ?
 
Have you consulted Sandvik? This sounds like their technology.
 