I have heard that there are charts available that correlate corrosion rates to temperature in the presence of sulfur compounds. Does anyone know where I could get my hands on such charts ?

Thanks in advance for any help !
 
For Sulfur without presence of Hydrogen see the McConomy curves. You can find them in Metals Handbook Volume "Corrosion"
 