Hello all
I am looking for suitable welding process for welding UNS N 8810 (Commonly called 800H). Is SMAW OK for weldig butt joints 12mm thk 810 material. What electrode should i go for.
This is in Flare system.
Are there some pit falls (in waiting) while qualifying
How about the bend test, would there be problems with that?
Are there any Corrosion test thatn are generally asked in this material (For this project there is no specific requirement) but i would rather have a procedure qualified with corrosion test so that in future if some other clients ask for Corrosion test i will already have some background info?
I am looking for suitable welding process for welding UNS N 8810 (Commonly called 800H). Is SMAW OK for weldig butt joints 12mm thk 810 material. What electrode should i go for.
This is in Flare system.
Are there some pit falls (in waiting) while qualifying
How about the bend test, would there be problems with that?
Are there any Corrosion test thatn are generally asked in this material (For this project there is no specific requirement) but i would rather have a procedure qualified with corrosion test so that in future if some other clients ask for Corrosion test i will already have some background info?