We need to replace a piece of equipment on our spray welder, it is called a bore attachment. It appears to be made from nylon, delrin or some type of plastic. It basically carries the welding wire and air through copper tubes down to the weld tip to reach into the bores of tubes etc. for welding. The area where the wires are attached have burned one side of the head. We have inquired to the manufacturer and the price is out of this world. If we could come up with a suitable material we would be farther ahead making it ourselves.

Assuming it was heat resistant and machinable. Not sure why we had the melting but have to assume it was caused by not properly connecting the lead from the welder since the other side is fine.

Any suggestions would be appreciated.

Dennis
 
Replies continue below

Recommended for you

Thanks for the response.

The head actually melted, the operator said he looked down and it was smoking. I don't think it is glass filled, not sure how to check. Both materials you referenced sounded interesting. The head is about 1-1/2" dia. x 5" lg. so were not talking about a very large part.

Dennis
 

Or "Torlo" if you can get it..polyamide-imide.


Cheers


Harry


 

Sorry, typo - should be "Torlon"
 
Thanks guys,

From what I can gather this doesn't seem to be glass filled. It has been turned in a lathe, milled, drilled and tapped. It's black and I would have to guess it has no fillers at all. It could be as simple as nylon or teflon. I think I'm going to look for something that might stand the heat better than our current part. I have it modeled and printed all I need now is to pick the material.

Thanks again,

Dennis

SolidWorks 2008 SP2
Windows XP Pro, Pentium4 3.00GHz
1GB RAM, Nvidia FX500
Logitech Marble Mouse, SpaceExplorer
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor