Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

sufficient corrosion allowance for 30 years pipeline 1

Status
Not open for further replies.

conero

Structural
Joined
Mar 15, 2001
Messages
1
Location
FR
In a pipeline 16 inch downstream a treatment I have a fluid
having the following carachteristic:

Stream Molar Component Percents
CO2 4.371 E-05 |
H2S 0.000 |
H2O 5.391 E-03 |
Design pressure 90 bar
temperature 50°C

Pipeline (long distance)
Design life 30 years
Material API 5L X65
MAOP(bara) 98
DesignFactor 0.72
Min. allow.thk 6.1(mm)
C.A. 1.00(mm)
Nominal thk 7.1(mm)
Burial Depth 0.9 m as minimum

May I consider the 1 mm sufficient for this dehydrated oil?
 
I would suggest that you model your line from a corrosion perspective. Flow rate, topography etc. One such company, with a great model is CorrosionWatch. I believe their website is or searh on the name.
Regards
 
I don't have the exact answer for this question. However, the external corrosion might be a serious problem for this underground piping system.

PAN
 