A friend of mine got the piston stuck up while he was pulling it out during major engine overhaul. He said that the engine was running ok before they started the overhaul. It seems that there was heavy carbon deposition on the liner that was not properly cleaned before they pulled the piston. The situation now that the piston is not moving neither up nor down. The engine is MaK marine engine model 16M453 rated 6000 hp. any clue on how to overcome this problem would be much appreciated. Regards WR...