By defination the stub ACME thread form has an included 29 degree angle. Does anyone have any experience in rounding slightly the upper crests of the thread to break the resulting shart corner?
How much rounding can you do and still conform to the standard?
Have male thread in F51 running in a female thread in 4130 (much softer). Concern is that the sharp edges of the male threads will bite into the female if there is any misalignment. Suggestion is to round the threads slightly to break the sharp corner, but QA has concerns that this will deviate from the standard thread form and will bear certification issues.
Thanks,
Andy
How much rounding can you do and still conform to the standard?
Have male thread in F51 running in a female thread in 4130 (much softer). Concern is that the sharp edges of the male threads will bite into the female if there is any misalignment. Suggestion is to round the threads slightly to break the sharp corner, but QA has concerns that this will deviate from the standard thread form and will bear certification issues.
Thanks,
Andy