Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations The Obturator on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Structural Steel Shapes

Status
Not open for further replies.

kevanthurman

Structural
Mar 25, 2009
11
Has anyone ever heard of a W14x17.2?

I have a set of building plans from 1968 and I believe one of the beams being called out is a W14x17.2.

I was wondering if this was a shape that used to be available or if anyone has an input on what is being called out please let me know.

I have attached the sheet where this beam is called out. It is the beam spanning from Grid 6 to Grid 9.
 
Replies continue below

Recommended for you

I can't take credit for this, although the drawing gave a big hint. I found this on the internet:



According to page 1-4 of AISC's "Manual" (6th Edition), 14B17.2 is classified as a "light beam", produced by Jones & Laughlin Steel Corp. From pages 1-22 & 1-23 for a designation 14x4B at 17.2 plf, section properties are listed as follows:

Ixx = 147.3, Sxx = 21.0, rx = 5.40, A = 5.05
Iyy = 2.65, Syy = 1.32, ry = 0.72
flange avg. thickness = 0.25"
web thickness = 0.1875"


Hope this helps,
Dave K. Adams, P.E.
Lane Engineers, Inc.
 
Neat! how did you get the file attachment?
Thanks, RAF
 
When you are posting, under step 3 where it says attachment click on the link to the right that says "...or upload your file to ENGINEERING.com". From there you can upload any file from your computer.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor