awa5114

Structural
Joined
Feb 1, 2016
Messages
135
Location
NL
Where can I find structural properties for AISI 316 steel? Specifically I am looking for Modulus of Elasticity, Shear Modulus, Poissons ratio, coefficient of thermal expansion, Density, Yield and Ultimate strength... I need to define this in RISA3D for a project....
 
If you are designing a stainless steel structure, I recommend AISC's Design Guide 27
E = 28,000 ksi
G = 0.385E
ν = 0.3
ε = 9.3 10-6/°F (for 68°-200° depends on temperature, Stl Const Manual list 9.9 for 18-8)
ρ = 500 pcf
Fy = 30 ksi (25 for 316L)
Fu = 75 ksi (70 for 316L)
 
Awesome. Thank you very much.
 