Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Structural glass design software ?

Status
Not open for further replies.

structuresguy

Structural
Apr 10, 2003
505
Do any of you know of any software packages for the structural design of sloped, non-rectangular glass windows subject to wind loading?

Thanks.
 
Replies continue below

Recommended for you

If you don't find other guide, I suggest you make analyses for your plate in FEM, and find rectangular ones that have the same deflection or maximum stresses. Basically you will get a relationship between the thicknesses that produce the same effect for one or other shape. Then the thickness of the worst "equivalent" rectangular one should be valid for your case.
 
Ya, that was basically what I was thinking. In fact, I have already done a model using plate elements in STAAD, but the material properties are not defined well. Depending where I look, I get widely varying Young's Modulus, from 9000-17000 ksi.

So making a decision on which one is difficult. Also, I don't know if tempering or heat treating affect the Young's Mod or not.

So I take the STAAD results with some skepticism, based on the unkwown material props.