I am looking for a coating/liner that can be utilized in a waste water stripping service. The waste water has an average pH of >12 s.u. and has high contents of metals. The metals are falling out in my stripper and causing under deposit corrosion. I have no means of adjusting the pH as the process results in elevated pH waste water. Most of my corrosion is occurring below the liquid level. I have been asked to review possible coating/liners available for a new waste water stripper. Does anyone know of any possible technologies availble for this service?
 