Howdy,

Does anyone know where I can find a stress strain curve for Al 6061-T4. I've been able to find 6061-T6 relatively easily, but T4 is giving me fits!

Thanks in advance!
PJF
 
Replies continue below

Recommended for you

Although you gave material and condition, shape, specification and thickness range were not given.
What can possibly be found are composite stress strain curves representing best fit of many tests, but it is probably questionable if they can be accepted as design data.

 
Well, let me be more specific....

6061-T4 Tubing: 0.028-0.035 inch thick
 