English-speaking countries refer to steel alloys that contain greater than ~ 10.5% chromium as "stainless steels". I am unclear what you mean by "mechaniced", however you need to provide additional information regarding the type of stainless steel you are using. Austenitic? Ferritic? Martensitic? Precipitation Hardening? If you have the chemical composition and/or specification (ASTM, EN, SAE, etc.) that would also be helpful.