Sep 12, 2000 #1 joker Industrial Joined May 26, 2000 Messages 2 Location US is it really necessary to stress relieve flame cut plate [sig][/sig]
Sep 12, 2000 #2 MikeMilburn Mechanical Joined Mar 22, 2000 Messages 115 Location CA It would depend on the type of plate, design of structure, and a lot of other variables...Mike [sig][/sig] Upvote 0 Downvote
It would depend on the type of plate, design of structure, and a lot of other variables...Mike [sig][/sig]
Oct 26, 2000 1 #3 vinod Electrical Joined Aug 20, 2000 Messages 6 To avoid cracking at edges it is better to stress relieve the flame cut plates to do so keep it in the sun for one month. or use a stress relieving furnace for temperature read ASME handbook Upvote 0 Downvote
To avoid cracking at edges it is better to stress relieve the flame cut plates to do so keep it in the sun for one month. or use a stress relieving furnace for temperature read ASME handbook
Jan 8, 2001 #4 fibretech Industrial Joined Jan 8, 2001 Messages 1 Location IN how can a heavy welded steel frame of a press can be stress relieved by heat treatment? how does it work? Upvote 0 Downvote
how can a heavy welded steel frame of a press can be stress relieved by heat treatment? how does it work?