Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Stress Relaxation In FEMAP with NASTRAN

Status
Not open for further replies.

jerzy

Mechanical
Joined
Aug 26, 2001
Messages
68
Location
US
Hello forum members,

I have been experimenting with creep analyses in FEMAP 10.3.1b with NASTRAN NX.
I have been using very simple models to gain insight into how the program works.
I create an analysis set in FEMAP and then use the "Preview Input" option to create two subcases
with different NLPARM statements, the first without creep, the second with CREEP time.

I have been using a model with a single ROD element using a material with CREEP prameters defined.
When I apply a constant force to this element, the results look reasonable: the first subcase gives
the non-creep response, and the second subcase gives larger and larger displacements when I increase the time value in the NLPARM statement.

I also try stress-relaxation cases where I impose a constant displacement on the ROD.
Here I get results I find puzzling. The first load case gives the expected ROD force for
a non-creep enforced displaceemnt, a tensile force for a stretching of the ROD element.
I would expect the second CREEP subcase to give a smaller tensile force as the stress relaxes in the element with the constant enforced displacement. Instead the ROD force changes sign and is given as a compressive force.

Has anyone done similar problems in FEMAP with NASTRAN NX and can furnish some observations about what is happening?

I started out wanting to study the behavior of bolted polymer flanges. I am trying to determine
how much of the initial bolt preload remains as the stress in the polymer flange relaxes over time.
I resorted to simple 1 or 2 ROD element models to gain insight into the CREEP routines.

Thank you

Jerzy
 