I have a formed C-channel with a 20k lb. load. Doing hand calculations I find the max stress should be 12,000psi. I calculated with an offset load. I then plugged everything into Mechanica and ran the FEA with a C-channel without radius from forming (To reduce the time to run) and found that I only have a large stress around 67,000psi on the corner of the channel where it welds to the girder. To see if the radii from the forming changed the results I added the radii and now have high stress of around 80,000 psi showing up near the formed radii under the load. Why am I seeing such a difference with just the radii being added? The results do not agree with my hand calculations also which makes me believe something is not modeled properly. Both ends of the girder are held in the x-axis but are able to rotate and move in the y-axis and the z-axis is able to rotate. The material is A572 Gr50 and I do not want to see over 28,000psi max stress.