NickE
Materials
- Jan 14, 2003
- 1,570
How sensitive is 17-7ph;C to strain rate?
We're currently making a part (stamped) and forming the shape in a real slow hydraulic press. We're about to gear up for production and want to use a stamper to form the shape. No stretch is being applied to the steel just a light bending. (15-45 degrees or so.
If my press head is moving roughly .167ft/sec.
Will I have to worry much?
Nick
We're currently making a part (stamped) and forming the shape in a real slow hydraulic press. We're about to gear up for production and want to use a stamper to form the shape. No stretch is being applied to the steel just a light bending. (15-45 degrees or so.
If my press head is moving roughly .167ft/sec.
Will I have to worry much?
Nick