Hi friends,

The firt time i hear about STRA test. Pls hepl me give your advice about this test.

STRA test is carried out to determine what?
 
The above refers to a specific orientation of a test sample for tensile testing to determine properties; tensile, elongation and reduction of area. Some refer to it as transverse tensile testing.
 