Stem material used A479Ty.410Cond.2/ A182GrF6aCl.3 due to higher yield strength, but customer wants only F6a Cl.2, what could be the reason please, Gate & Globe Valves
 
The question is for your customer to answer...What valve are you discussing ?

Per ISO, only the term Safety Valve is used regardless of application or design.
 