Please relate any experience on damage mechanisms to Stellite 6 on valve seats and plugs if the valves are passing subcooled water at 300 degrees C and 155bar? The downstream side of the valve is at STP thus the liquid flashes to steam. The environment is typical to a nuclear 900MW PWR reactor primary circuit Power Operated Relief Valve.
 
Replies continue below

Recommended for you



you need to be more specific about the valve you are using, it is not a service that merits a generic answer
 
While Stellite 6 and other numbers are very erosion-resistant, they sure aren't erosion-proof. Your conditions are severe.

BTW, since you're dealing with the primary-side, don't you have concerns with cobalt-reduction in valves (for radiation reduction)?
 