Hi i have a client who has Mills that turn out fence poles.
the start product is a bar 120x120 mm in size. He needs to de-scale it moves at 2 m per sec is 1000 deg c in temp.
Any assistance would help.BUT Please cost is a factor.
Thanks
Robert
 
Hi Thanks


Reply
E-mail It
ferreiro (Mechanical) Mar 25, 2002
Hi i have a client who has Mills that turn out fence poles.
the start product is a bar 120x120 mm in size. He needs to de-scale it moves at 2 m per sec is 1000 deg c in temp.
Any assistance would help.
Thanks
Robert


DayDesign


D
 
I assume that this is for a mini-mill.

What type of steel is being processed and at what temperature? I am assuming low to high carbon steels at 2400F.

Does your client currently have descaling capability? Most of these systmes are at 3000psig and use multiple stage pumps such as Union.

These systems are simple but require high pressure and strained water. There are many types of circular spray rings available. Try Spraying Systems.

Dennis H. Radford
 