I am in search of a paint that can be applied to steel and can be removed in ~10% hydrochloric Acid at 180 degrees(C) in ~2 minutes.
To add some information the paint that we apply at approximately 600 degrees (C), comes off perfectly in the acid described above, I believe this is because the polymers that are in the paint vapourize when reaching temperatures of >400 degrees (C).
Note:Hydrochloric acid is very reactive with metallics and not reactive with anything that is hydrocarbon based.