steel grain?

Status
Not open for further replies.

structSU10

Structural
Mar 3, 2011
1,062
I am reviewing some calculations and there is this general note:

"Orient steel grain structure perpendicular to bend lines for all bent plates used as connection material..."

Anyone know the reason for this? I never heard of any issue with orientations of a steel plate prior to bending.
 
Replies continue below

Recommended for you

I think plate material has a "grain" from the rolling process. I think the Green Book has some commentary on this.
I believe there is different min. bend radii depending on which way you are bending...with or across the "grain".
 
Toad is right, the rolling process does tend to cause a grain orientation in the steel. When this rolling grain orientation is parallel to the bend line the plate does have a tendency to rip or split, on the tension side, along the bend line. Thus, you may have to increase the bending radius as AISC suggests. You can bend to a tighter radius when the grain runs perpendicular to the bend line, a more favorable tensile orientation. Any edge nicks and the like can cause problems in either direction so it is common to dress the edges of a plate a little at the bend lines.
 
That makes sense, good to know, thanks for the replys!
 