Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

steel for cutting spring wire sae 1070

Status
Not open for further replies.

pardal

Automotive
Joined
Oct 17, 2001
Messages
444
Location
AR
I need to build a cuting die to split coiled spring wire
1,75 mm diameter.MATERIAL IS sae 1070
The female die is a cilinder 56 mm diam , the female wide is 28 mm .
The purpouse is to cut in two parts each turn in one stroke, 10 turns of the coiled spring to get retaining ring .
I have the drawing if needed.
Pardal
 
Is the spring wire to be cut already heat treated to a spring temper? In other words, what is the strength and hardness of the wire to be cut? If it is already heat treated to a high hardness, then you will probably need a tungsten carbide-type material for optimum cutting (minimum burr, suitable cutting life, etc.). If it is annealed, then you can probably use a tool steel.
 
The wire is as I bougth it , in roll .I coil it to 56 internal diameter as a extension spring.
Ther is no previous heat treatment.
I get some info that recomend to use D2 tool steel , hardend, and tempered to 56 60 HRC.
If the wire is 1,75 mmm and using such steel , what is the gap between male and female?
Thanks for your advice.