I am searching for the Chinese equivalent for SAE 1035. Please help me if you know how to find this.
 
Grade 35 according to GB 699 is the equivalent of SAE 1035. The best sources for this type of information are reference books available from ASM International. The following thread has links to the various ASM products:

thread330-93855
 