Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations The Obturator on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Steel Column to Beam Connection 1

Status
Not open for further replies.

mjohan

Structural
Dec 7, 2002
91
Should there be a different type of connection for a column base plate to a W shaped top flange; when the beam is in positive moment, when the beam is in negative moment?

I would like to use a steel base plate with 3/4" bolts connecting to the top flange. I am concerned with:

1) The reduction in area of top flange while the beam is in negative moment.

2) If eliminating the bolts, would welding the base plate to the top flange result in an undesirable connection while the beam is in negative moment?

I appreciate any help on this subject.
 
Replies continue below

Recommended for you

mjohan,

AISC allows to use the gross area of the section if
0.5 Fu Anet >= 0.6 Fy Agross.
That applies to both, the tension and compression flanges.

To weld the base plate to the beam is also acceptable. The welding should be done correctly, of course, to reduce the stresses that the heating and cooling of the welds could introduce.

Regards
 
mjohan,

I forgot to include the pertinent paragraphs from the AISC - ASD: B2, B3 and B10
 
Just curious, how do you have top and bottom flange on a column?
 