Would anyone be kind to help me identifying any US / NACE standard or perhaps european norm, the equivalent of Australian Standard AS 2832.4-2006 (Cathodic Protection of metals - Part 4: Internal surfaces) and AS 2239-2003 (Galvanic sacrificial anodes for cathodic protection). I have to nominate an acceptable international design standard for the sacrificial cathodic protection of a carbon steel process vessel containing some weak electrolyte fluid, where the internal coating is not an option.

Thanks in advance

gr2vessels
 
API-651 - Cathodic Protection of Aboveground Petroleum
Storage Tanks

BS 7361 Part 1 1991 'Cathodic Protection Part 1 - Code of
Practice for Land and Marine Applications' British Standards
Institution, U.K.

NACE Standard RP0196-2004
Title: Galvanic Anode Cathodic Protection of Internal Submerged Surfaces of Steel Water Storage Tanks
 
Thanks Chris,

Good advice.

Cheers,

gr2vessels
 