Is there information and/or a book on dimensional tolerances
for Plastics?
 
What process are you looking for information on? injection molded plastics, machining plastics or some other process.

Best Regards,

Heckler
Sr. Mechanical Engineer
SW2005 SP 3.1 & Pro/E 2001
Dell Precision 370
P4 3.6 GHz, 1GB RAM
XP Pro SP2.0
NIVIDA Quadro FX 1400
o
_`\(,_
(_)/ (_)

"There is no trouble so great or grave that cannot be much diminished by a nice cup of tea" Bernard-Paul Heroux

 
Injection molded plastics.
 
Designing with Plastics and Composites Handbook & Modern Plastics Handbook are two books I use.

Best Regards,

Heckler
Sr. Mechanical Engineer
SW2005 SP 3.1 & Pro/E 2001
Dell Precision 370
P4 3.6 GHz, 1GB RAM
XP Pro SP2.0
NIVIDA Quadro FX 1400
o
_`\(,_
(_)/ (_)

"There is no trouble so great or grave that cannot be much diminished by a nice cup of tea" Bernard-Paul Heroux

 
Thanks for your help. I found another one from SPI.
Standards & Practices of Plastics Molders.
 
ag6533-
Be careful about tolerances published by trade organizations such as these! They tend to publish tolerances that are VERY conservative. For example, the RMA (Rubber Manufacturer's Association) lists tolerances that are so coarse that one is tempted to rule out that family of materials. Another fine example is NADCA (North American Die Casters Association). I discovered that the best source of information on D&T of injection molded parts is a knowledgeable, cooperative injection molder!