Does anyone know where I can find a list of AWS's standard finishing designations? For example, G = Grinding, C = Chipping, and M = Machining. Are there any other types? See attached for clarification (in blue). Thanks in advance.

- Adam
 
Replies continue below

Recommended for you

3.13 in AWS 2.4. The 98 version just shows 5, chipping, grinding, hammering, machining, rolling, plus U for Unspecified.
 