Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Standard welded Fitting in Pressure vessel

Status
Not open for further replies.

Cleandive

Mechanical
Joined
Aug 3, 2014
Messages
12
Location
CA
When the standard b 16.9 fitting has long seams, for using such a standard Fitting in Pressure vessel,is it required for the pressure vessel manufacturer to obtain the WPS and PQR and get it reviewed by AI and include in the final dossier, also is PQR for the fitting required to take into account the possible PWHT cycle that the fitting may under go during PWHT of the vessel. If Fitting PQR is required to take care of future PWHTs, then how many cycles are required to be considered from ASME Sec VIII Div 1 point of view (not from any client specification please).

A) Fitting is A 234 WPB
B) fitting is A 420 WPL 6

 
You need to comply with all the requirements of UG-11(c)
WPS used must have been qualified with the PWHT cycle for the vessel. PWHT time at temperature is a supplementary essential variable and if impact tests are not required, PWHT time is not a variable.
Future PWHT during service are not addressed by Section VIII Division 1.
You will need to obtain the radiographs from fitting manufacturer
Records are required to be retained as required by App 10-13 (pressure part documentation and certification)
Ofcourse you should discuss with your AI
 
Cleandive,
You wrote:
"for using such a standard Fitting in Pressure vessel"

Could you please explain what you mean by this?

Sometimes its possible to do all the right things and still get bad results
 
If te fitting was welded with added weldmetal you will need a partial data report and if pwht in the specification a pwht certification as well.no need for PQR or WPS. If no addition of weldmetal as ERW welding, only certifications mby the part mfr will be required to comply with the specification.
 
Dear GenB
Partial data report is not required for standard fittings. Please refer UG-11(c)
Ofcourse all other requirements of UG-11(c) must be met
 
Please read UG 11 (c)5,Standard parts are not required with partial data reports.
 
can somebody help me with this code