Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Standard Lengths of W Shape I beams

Status
Not open for further replies.

TCPhoenix

Mechanical
Jan 23, 2007
24
I am using some W12x50's and W12x58. What is the standard lengths i can buy these in?
 
Replies continue below

Recommended for you

Check with a steel supplier. I think they come in 40' and up to 60'. Size is usually limitted by waht can be shipped/trucked.
 
40' and 60' lengths are fairly 'standard' in my area (Nebraska). These are the lengths likely to be sitting in the fabricator's on hand stock piles, or at steel warehouses.

Longer lengths can be specially ordered, but these take time to acquire.
 
A fabricator once told me that if I tried to keep my lengths as close to multiples of 5'-0" and not over ended up with less waste for him. He orders his sections in lengths like 50', 55', 60' etc, so when I used a piece that was 61'-4" long, it required him to waste 3'-8" a bunch of times.
 
I think we can usually get 40', 50', and 60'. And of course if you need more than one, that gives you 20', 25', and 30' lengths. If you need large quantities, you can get mill orders in custom lengths.
 