Stain from Fireproofing crack

Status
Not open for further replies.

MATEGRITY2009

Petroleum
Oct 9, 2009
43
Hi all,


During PFP vessel survey we found this stained from cracking on PFP and PEC test over the cracking PFP and nearest section found no corrosion under fireproof.


Anyone experience this problem, please advise. for me it look like some grease but i'm not sure this is from fireproof build process or what??

 
Status
Not open for further replies.