St. 52-3 U (1.0553) – S355J0
S: Structural Steal
J0: 27 Joule for testing temp 0 DegC (Nom. Thick. >10 / <=150 mm)
Yield ReH: 275 – 355 MPa
Tensile Rm: 450 – 680 MPa
St. 52-3 N (1.0570) – S355J2G3
S: Structural Steal
J2: 27 Joule for testing temp -20 DegC (Nom. Thick. >10 / <=150 mm)
G3: Normalised
Yield ReH: 275 – 355 MPa
Tensile Rm: 450 – 680 MPa
Lowest values are for the lowest value of the thickest section available.
Heist values are for the heist value of the thinnest section (<3 mm for Rm, <=16 mm for ReH)