One of our customers wants the additional requirements for SA 516-70N materials. But I can not find any dealer or mill can offer it.
1. Are these SSC and HIC test method suitable for SA 516-70N?
2. Are these requirements difficult to meet for SA 516-70N?
3. Is there any one can provide some test result about SSC, HIC for SA 516-70N using the flowing method?
------ FOLLOWINGS ARE MATERIALS SPECIFICATION ------
- PLATE 1.75”THK x 120”W x 370”LG SA 516-70N
- PLATE 1.75”THK x 142”W x 142”LG SA 516-70N
Materials shall, in addition to meeting the requirements of ASTM A 516 70N, satisfy the following criteria and standards:
1. CHEMICAL COMPOSITION
1.1 % Sulphur: 0.003% max (heat and product analysis)
1.2 % Phosphorous: 0.015% max (heat and product analysis)
1.3 CE: 0.43 max
2. MECHANICAL TEST
2.1 Impact test @ -45ºC
2.2 Drop-weight test shall be towards ASTM E 208, and based upon the proposed minimum design temperature, -45ºC
3. Ultrasonic examination as per SA 587-C
4. Magnetic particle examination
5. Parent material and weldment shall comply with the requirements of Clause 7 and SSC Region 2, as shown in Figure 1 of NACE MR0175 / ISO 15156 Part 2. Microhardness shall be maximum 248HV500 (ASTM E 384) and macrohardness maximum 22HRC (ASTM E 18).
6. SSC resistance shall comply with Annex B of NACE MR0175 / ISO 15156, and as follows:
a. Laboratory testing shall satisfy tests for specific sour service application in accordance with Clause B.3 of Annex B.
b. Test requirements shall be in accordance with NACE TM0177, performed at a temperature of 24oC±3oC (75oF±5oF).
c. The test qualification validity shall be in accordance with Table B.1, SSC Region 2, test type FPB, applied stress > ?> 90% AYS, pH of the environment shall be adjusted to 4. FPB test shall be in accordance with Appendix 2 of EFC Publication No. 16, ISO 7539 Part 2. FPB evaluation and acceptance criteria shall meet with the requirements of B.4.2.3, Annex B of NACE MR0175 / ISO 15156 Part 2 for SZC and SOHIC.
d. The test environment shall be,
i. 5% mass fraction NaCl + 0.4% mass fraction CH3COONa.
ii. pH 4, adjusted using HCl or NaOH.
iii. H2S partial pressure 9.7KPa or alternatively 2,300ppm after saturation of the environment.
e. The acceptance criterion is, no cracking.
7. HIC and SWC resistance shall comply with the requirements of B.5 and Table B.3 of Annex B of NACE MR0175 / ISO 15156 Part 2, and as follows:-
a. Testing shall be in accordance with NACE TM0284. Testing temperature shall be 25ºC±3ºC (77ºF±5ºF).
b. The test environment shall be the same as in 6.d above.
c. The acceptance criterion is, no cracking.
1. Are these SSC and HIC test method suitable for SA 516-70N?
2. Are these requirements difficult to meet for SA 516-70N?
3. Is there any one can provide some test result about SSC, HIC for SA 516-70N using the flowing method?
------ FOLLOWINGS ARE MATERIALS SPECIFICATION ------
- PLATE 1.75”THK x 120”W x 370”LG SA 516-70N
- PLATE 1.75”THK x 142”W x 142”LG SA 516-70N
Materials shall, in addition to meeting the requirements of ASTM A 516 70N, satisfy the following criteria and standards:
1. CHEMICAL COMPOSITION
1.1 % Sulphur: 0.003% max (heat and product analysis)
1.2 % Phosphorous: 0.015% max (heat and product analysis)
1.3 CE: 0.43 max
2. MECHANICAL TEST
2.1 Impact test @ -45ºC
2.2 Drop-weight test shall be towards ASTM E 208, and based upon the proposed minimum design temperature, -45ºC
3. Ultrasonic examination as per SA 587-C
4. Magnetic particle examination
5. Parent material and weldment shall comply with the requirements of Clause 7 and SSC Region 2, as shown in Figure 1 of NACE MR0175 / ISO 15156 Part 2. Microhardness shall be maximum 248HV500 (ASTM E 384) and macrohardness maximum 22HRC (ASTM E 18).
6. SSC resistance shall comply with Annex B of NACE MR0175 / ISO 15156, and as follows:
a. Laboratory testing shall satisfy tests for specific sour service application in accordance with Clause B.3 of Annex B.
b. Test requirements shall be in accordance with NACE TM0177, performed at a temperature of 24oC±3oC (75oF±5oF).
c. The test qualification validity shall be in accordance with Table B.1, SSC Region 2, test type FPB, applied stress > ?> 90% AYS, pH of the environment shall be adjusted to 4. FPB test shall be in accordance with Appendix 2 of EFC Publication No. 16, ISO 7539 Part 2. FPB evaluation and acceptance criteria shall meet with the requirements of B.4.2.3, Annex B of NACE MR0175 / ISO 15156 Part 2 for SZC and SOHIC.
d. The test environment shall be,
i. 5% mass fraction NaCl + 0.4% mass fraction CH3COONa.
ii. pH 4, adjusted using HCl or NaOH.
iii. H2S partial pressure 9.7KPa or alternatively 2,300ppm after saturation of the environment.
e. The acceptance criterion is, no cracking.
7. HIC and SWC resistance shall comply with the requirements of B.5 and Table B.3 of Annex B of NACE MR0175 / ISO 15156 Part 2, and as follows:-
a. Testing shall be in accordance with NACE TM0284. Testing temperature shall be 25ºC±3ºC (77ºF±5ºF).
b. The test environment shall be the same as in 6.d above.
c. The acceptance criterion is, no cracking.