SS vs SST

Status
Not open for further replies.

g30rg3

Mechanical
Joined
Nov 9, 2014
Messages
5
Location
AE
Could some one give me an insight as to what is the difference between "SS & SST" in terms of stainless steel material ie 416 SS & 416 SST.

My first instinct was that they were the same both SS and SST stands for stainless steel, just written in a fancy manner.

I may be wrong. If you feel so it would be great to know.

Thank you for your time.

veneeth george
piping engineer - offshore rigs
 
They are one in the same abbreviation. It should be listed as Type 416 with no suffix.
 
metlonis - that post was an interesting read.
metengr - that make sense

Thank you for your time.
 
My response would be AO.

Which stands for Acronym Overload.