Hai Guys,

I need to qualify WPS for SS Weld Overlay in 4130 material.We are using SMAW & MIG also..Which type of electrodes are using in this process..I think For SMAW Electrode should be E 309 Mol-16 + E 316l-17....Is it Right or not?
Can anyone suggest me the mig filler wire for SS Overlay in 4130 material
 
Replies continue below

Recommended for you

Yes, look at AWS SFA 5.9. Are you depositing 316L as the corrosion resistant overlay (CRO)? What code are you working under for qualification of the WPS? The reason is that for CRO certain codes have specific requirements for qualification of the welding procedure.
 
Hi,

I am following asme sec ix..Can you suggest me the MIG filler wire used for ss weld overlay in 4130 material.
 
The GMAW process will produce a higher hardness in the 4130 material. Take extra precaution regarding preheat for the initial layer.
 