Hello everyone, I'm looking for the composition of an alloy known as WC 6 used for high temperature applications(1000 deg. C).

Regards
 
1 1/4 Cr 1 Mo Steel casting Material

UNS J12072

Vita sine litteris mors est.
 
Possibly Tungsten Carbide??? We used to thermally spray it as a "Hardface" surface on turbine blades
 
Thanks to Rich2001 and Capntom.

I believe it is UNS J12072 because it is a steel casting. I should have mentioned that in my original post, my apologies.

Cheers
 