Jul 25, 2005 #1 macmet Materials Joined Jul 18, 2005 Messages 863 Location CA Hello everyone, I'm looking for the composition of an alloy known as WC 6 used for high temperature applications(1000 deg. C). Regards
Hello everyone, I'm looking for the composition of an alloy known as WC 6 used for high temperature applications(1000 deg. C). Regards
Jul 25, 2005 #2 Rich2001 Mechanical Joined Mar 23, 2001 Messages 896 Location US 1 1/4 Cr 1 Mo Steel casting Material UNS J12072 Vita sine litteris mors est. Upvote 0 Downvote
Jul 25, 2005 #3 Capntom Mechanical Joined May 22, 2003 Messages 63 Location US Possibly Tungsten Carbide??? We used to thermally spray it as a "Hardface" surface on turbine blades Upvote 0 Downvote
Jul 25, 2005 Thread starter #4 macmet Materials Joined Jul 18, 2005 Messages 863 Location CA Thanks to Rich2001 and Capntom. I believe it is UNS J12072 because it is a steel casting. I should have mentioned that in my original post, my apologies. Cheers Upvote 0 Downvote
Thanks to Rich2001 and Capntom. I believe it is UNS J12072 because it is a steel casting. I should have mentioned that in my original post, my apologies. Cheers