Currently use a chrome plated formed bar which is 1/2" dia carbon steel with both ends bent down 90 degrees and flattened with holes in the turned down ends. The flattened end is approx. 1/4" thick. This is a tooled part and is chrome plated after forming.
Would like to try some type of SS bar that could be formed and used without plating.
What type and condition of SS would most likely withstand the bending and flattening and hopefully use the existing tooling?
Thanks,
Would like to try some type of SS bar that could be formed and used without plating.
What type and condition of SS would most likely withstand the bending and flattening and hopefully use the existing tooling?