May 22, 2018 #1 Water Mamba Petroleum Joined May 22, 2018 Messages 2 Location US What section in ASME Section VIII div.1, requires Spot RT on BW with 10" OD and greater?
May 22, 2018 #2 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,863 Location US None at all, unless in special services. See UW-2. Otherwise, degree of RT generally a decision made by the designer. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand Upvote 0 Downvote
None at all, unless in special services. See UW-2. Otherwise, degree of RT generally a decision made by the designer. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand
May 22, 2018 Thread starter #3 Water Mamba Petroleum Joined May 22, 2018 Messages 2 Location US Clarification 10" Diameter nozzle BW? Upvote 0 Downvote
May 23, 2018 #4 marty007 Mechanical Joined Mar 8, 2012 Messages 622 Location CA Read paragraph UW-11(b), it provides exemptions for nozzle welds of certain sizes. Upvote 0 Downvote
May 23, 2018 #5 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,863 Location US See also UW-11(a)(5)(b) Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand Upvote 0 Downvote
See also UW-11(a)(5)(b) Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand