What section in ASME Section VIII div.1, requires Spot RT on BW with 10" OD and greater?
 
None at all, unless in special services. See UW-2. Otherwise, degree of RT generally a decision made by the designer.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Read paragraph UW-11(b), it provides exemptions for nozzle welds of certain sizes.
 
See also UW-11(a)(5)(b)

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 