Good afternoon all,

Can anyone provide some guidelines for specifying pumps for use in sour water service?

I am looking into a 561 GPM, 280 feet of water pump that will be pumping 0.92 wt% H2S and 0.64 wt% NH3.

I am looking for any tips, but in particular for materials of construction, mechanical seal types, etc. Thanks in advance.
 
Replies continue below

Recommended for you

Also, temperature will be 150 deg F.
 