Apr 7, 2003 #1 AllenMueller Mechanical Joined Apr 7, 2003 Messages 1 Location US Does any one know a sound absorption coefficient for polypropylene plastic? I'm just looking for an estimate so any help would be great. Thanks in advance
Does any one know a sound absorption coefficient for polypropylene plastic? I'm just looking for an estimate so any help would be great. Thanks in advance
Apr 9, 2003 #2 okdb Mechanical Joined Feb 11, 2003 Messages 45 Location NO Hi, In what form is your plastic? in sheat, foam, loose microballs? To have any absorption properties, your product has to be foam with open cells. cheers, OkdB Upvote 0 Downvote
Hi, In what form is your plastic? in sheat, foam, loose microballs? To have any absorption properties, your product has to be foam with open cells. cheers, OkdB
Apr 13, 2003 #3 pheon Mechanical Joined Apr 13, 2003 Messages 12 Location US The sound absorption coefficient of plastic materials is also frequency dependent. Upvote 0 Downvote