WeldGk
Materials
- Aug 14, 2007
- 42
Can anyone advise as to the reason that API does not accept the continuous process annealing for 316 stainless? API is stipulating that the time is a requirement but most mills do not provide a specific time as the annealing is carried out in a continuous fashion.