roniprabowo
Mechanical
Dear all,
We have bought plate material to fabricate tank with carbamate solution service.
Plate material is SA-240 Typ 304. Is it mandatory for mill supplier to do solution annealed ?
As far as I know this requirement is clearly stated in ASTM and I do not see this test being done in mill certificate.
Looking forward for this information.
We have bought plate material to fabricate tank with carbamate solution service.
Plate material is SA-240 Typ 304. Is it mandatory for mill supplier to do solution annealed ?
As far as I know this requirement is clearly stated in ASTM and I do not see this test being done in mill certificate.
Looking forward for this information.