Hi,

I need data (x-y graph) for solubility of SO2 in concentrated sulphuric acid (approx. 98%) at temperature approx. 80 deg. C.
Can anyone send me this data or give a link/reference?

Thanks in advance for any help,
Paul

PS. If not solubility, it may be partial pressure of SO2 over SO2 solutions in H2SO4 - I'm not sure which name is more accurate.
PS2. I'm sorry for double-posting (in another part of this forum) but it's very important and I hope that more people will see my post in this section.
 
If you can't find anything free, the following shows data you can buy from the Detherm databank at

best wishes,
sshep

The first number is the number of lines of data, the second number is the price (i.e. 80.00=$80):

Lines USD property - click icon for preview system year T P
22 80.00 concentration solvent,solubility sulfur dioxide/sulfuric acid/water 1975 293 K- 313 K 31197 Pa-189718 Pa
23 80.00 Gas solubility data sulfur dioxide/sulfuric acid/water 1920 293 K 101325 Pa
9 50.00 Gas solubility data sulfur dioxide/sulfuric acid/water 1934 298 K 132 Pa- 1036 Pa
24 80.00 Gas solubility data sulfur dioxide/sulfuric acid/water 1997 298 K 33 Pa- 864 Pa
23 80.00 Gas solubility data sulfur dioxide/sulfuric acid/water 1928 314 K- 335 K 101325 Pa
22 80.00 Gas solubility data sulfur dioxide/water/sulfuric acid 1975 293 K- 313 K 31197 Pa-189718 Pa
27 80.00 Gas solubility data sulfur dioxide/water/sulfuric acid 1956 283 K- 305 K 152 Pa- 3546 Pa
 