Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Software CO2/H2S gas wells corrosion rate prediction

Status
Not open for further replies.

Peter113

Materials
Joined
Oct 17, 2007
Messages
19
Hello to all,
would you recommend me a software related material selection for line pipe on sweet and sour service?
regards
Peter
 
Peter

There are some good software for Corrosion prediction in sweet and sour service.
The Norsok software is free, but is limited to a Sweet service, there is a limit on the max H2S. You can download it at:

Then there are others software that you can try and buy.
The electronic engineer from intetech can take into account also the effect of h2s on corrosion:

hope this help u