Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SO2 Line Clogging

Status
Not open for further replies.

doomster

Chemical
Joined
Feb 4, 2019
Messages
45
Location
PH
We have a recurring situation in our Selenium roaster, we feed SO2 to reduce selenium. The SO2 that we're using is a liquid cylinder SO2. We use a steam vaporizer to vaporize liquid SO2. Now the problem is that SO2 line always clogging. What could have cause this?

 
What is MOC of the transport line? Can't a sample of the plugging agent be analyzed?
 
Is the steam at a higher pressure than SO2 in the vaporiser? If so, could steam be leaking into the SO2 side of the vaporiser( through a broken vaporiser tube or tube-tubesheet joint??), making the now wet SO2 very corrosive to the downstream piping ? Ask for a hydrotest of the vaporiser.
 