Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Small penetrations in existing concrete slabs 1

Status
Not open for further replies.

jtstruct

Structural
Jun 20, 2003
21
Do any of you know of "rules of thumb" available for small penetrations of existing concrete floor slabs? I have a condition where they would like to drill a small conduit (3/4") through an elevated cast-in-place floor slab (old building), or possibly drill a 3/4" groove in the top of the slab for a length of 3'. This got me thinking about wood design and typical requirements for joist penetrations - notching or drilling in relationship to the proximity of the bearing, depth of joist, length of span, etc.

Are there similar types of informal guidlines for concrete slab penetrations that you all are aware of? Any references would be greatly appreciated.

Thank you.
 
Replies continue below

Recommended for you

A 3/4" hole in the concrete isn't going to hurt anything to any significant degree.

The groove might be a bit more of a problem by creating a potential crack line. It could also reduce the load carrying capacity of the slab in that immediate area. I'd be more concerned about the groove...it depends on where the groove is relative to the slab span.
 
JAE... have to watch out for those nasty prestressing cables <G>...
 
dik - right on with the prestress! - I agree that that would be real BAD to hit one of those.

He did say &quot;old buildling&quot; so I just assumed it was mild steel.
 